Cross-linked poly(α,ω-bis(3-pyrrolyl)alkanes) were directly applied to woven wool substrates by either chemical, vapour or mist polymerization methods. Choice of dopant could greatly improve the surface resistance. The optimum coating on textiles with the lowest surface resistance, highest colour-fastness and stability was achieved using a mist polymerization method with 1,8-bis(pyrrolyl)octane, iron(III) chloride (FeCl3) as the oxidant and p-toluene sulfonic acid sodium salt (pTSA) as the dopant.