Effect of processing parameters on the magnetic properties and macrotexture of a Nd13.5Fe73.8Co6.7B5.6Ga0.4 alloy processed by equal channel angular pressing with back pressure

Onal, E., Lapovok, R., Kishimoto, H., Kato, A., Davies, C. H. J. and Suzuki, K. 2016, Effect of processing parameters on the magnetic properties and macrotexture of a Nd13.5Fe73.8Co6.7B5.6Ga0.4 alloy processed by equal channel angular pressing with back pressure, IEEE transactions on magnetics, vol. 52, no. 7, pp. 1-4, doi: 10.1109/TMAG.2016.2529602.

Attached Files
Name Description MIMEType Size Downloads

Title Effect of processing parameters on the magnetic properties and macrotexture of a Nd13.5Fe73.8Co6.7B5.6Ga0.4 alloy processed by equal channel angular pressing with back pressure
Formatted title Effect of processing parameters on the magnetic properties and macrotexture of a Nd13.5Fe73.8Co6.7B5.6Ga0.4 alloy processed by equal channel angular pressing with back pressure
Author(s) Onal, E.
Lapovok, R.
Kishimoto, H.
Kato, A.
Davies, C. H. J.
Suzuki, K.
Journal name IEEE transactions on magnetics
Volume number 52
Issue number 7
Start page 1
End page 4
Total pages 4
Publisher IEEE
Place of publication Piscataway, N.J.
Publication date 2016-07
ISSN 0018-9464
Summary Equal channel angular pressing (ECAP) is a well-established thermo-mechanical processing technique, which could induce the c-axis texture of Nd2Fe14B in a melt-spun Nd13.5Fe73.8Co6.7B5.6Ga0.4 alloy. However, the effects of ECAP processing parameters, such as temperature, back pressure (BP), and multiple-pass ECAP routes, remain unknown for this alloy. In this paper, we have investigated the effects of these processing parameters on the c-axis texture formation. It is found by X-ray diffraction macrotexture analysis that the maximum intensity of (001) pole figures for the tetragonal-Nd2Fe14B phase (Imax) shows an increase from 2.7 to 4.1 m.r.d. (multiples of random distribution) by increasing the ECAP temperature from 723 to 823 K, while the difference in remanent magnetization between easy and hard directions (Δ Mr) rises from 24.0 to 41.5 Am2/kg. When the BP was increased from 0.25 to 0.5 GPa at 823 K, Imax showed an increase from 2.8 to 4.1 m.r.d. However, Imax saturated for BPs above 0.5 GPa, suggesting that BP has limited effect on the texture formation, although it is necessary for the compaction of the alloy powders. Two multiple-pass ECAP routes conventionally known as routes A and C were employed for two-pass ECAP at 823 K. It is found that route A processing is effective in enhancing the texture formation, while the texture is lost by a subsequent pressing when adopting route C. Therefore, the compaction of Nd13.5Fe73.8Co6.7B5.6Ga0.4 alloy powder using route A ECAP passes with 0.5 GPa BP at 823 K results in pronounced texture, which is beneficial for anisotropic hard magnetic properties.
Language eng
DOI 10.1109/TMAG.2016.2529602
Field of Research 02 Physical Sciences
09 Engineering
091207 Metals and Alloy Materials
Socio Economic Objective 970109 Expanding Knowledge in Engineering
HERDC Research category C1 Refereed article in a scholarly journal
ERA Research output type C Journal article
Copyright notice ©2016, IEEE
Persistent URL http://hdl.handle.net/10536/DRO/DU:30085080

Document type: Journal Article
Collection: Institute for Frontier Materials
Connect to link resolver
 
Unless expressly stated otherwise, the copyright for items in DRO is owned by the author, with all rights reserved.

Versions
Version Filter Type
Citation counts: TR Web of Science Citation Count  Cited 0 times in TR Web of Science
Scopus Citation Count Cited 0 times in Scopus
Google Scholar Search Google Scholar
Access Statistics: 69 Abstract Views, 1 File Downloads  -  Detailed Statistics
Created: Tue, 26 Jul 2016, 08:55:01 EST

Every reasonable effort has been made to ensure that permission has been obtained for items included in DRO. If you believe that your rights have been infringed by this repository, please contact drosupport@deakin.edu.au.