A microstructure-based creep model for additively manufactured nickel-based superalloys

Version 2 2024-06-04, 12:11
Version 1 2023-10-23, 23:06
journal contribution
posted on 2024-06-04, 12:11 authored by S Wu, HY Song, HZ Peng, Peter HodgsonPeter Hodgson, H Wang, XH Wu, YM Zhu, MC Lam, AJ Huang
A microstructure-based creep model for additively manufactured nickel-based superalloys