posted on 2010-01-01, 00:00authored byChengpeng Li, J P Zhong, L Yang, S D Li, Lingxue KongLingxue Kong, T T Hou
To evaluate calcium chloride coagulation technology, two kinds of raw natural rubber samples were produced by calcium chloride and acetic acid respectively. Plasticity retention index (PRI), thermal degradation process, thermal degradation kinetics and differential thermal analysis of two samples studied. Furthermore, thermal degradation activation energy, pre-exponential factor and rate constant were calculated. The results show that natural rubber produced by calcium chloride possesses good mechanical property and poor thermo-stability in comparison to natural rubber produced by acetic acid.
History
Journal
E-polymers
Volume
072
Pagination
1 - 9
Location
[Strasbourg, France]
Open access
Yes
ISSN
1618-7229
Language
eng
Notes
Reproduced with the specific permission of the copyright owner.