Two-dimensional tungsten disulphide flakes are developed via a two solvent grinding assisted liquid phase exfoliation method. Our investigations show the distinct advantages of this approach that include reduced residues of the solvent used, high yield and creating relatively thin flakes suitable for electronic, optical, catalytic and energy storage applications.