Initiation of plasticity by nanoindentation in Mg alloys

Download (44.08 MB)
thesis
posted on 2015-10-01, 00:00 authored by T Guo
In this study, nano-indentation technique is employed to investigate the initiation of basal slip and extension twin separately in magnesium. The present method prove useful in studying the influence of solid solution and precipitates on these two deformation modes.